Hot-Weather Concreting (>27°C): Preventing Slump Loss & Plastic Shrinkage Cracking
Category: Ready-Mix Concrete
Summer heat waves, low humidity, and afternoon winds across Southern Ontario create high-risk conditions for concrete placement. Under CSA A23.1:24, hot-weather concreting controls trigger whenever ambient air temperature reaches or is forecast to exceed 27°C during placement.
What High Heat Does to Fresh Concrete
When concrete temperatures climb above 30°C–32°C, hydration accelerates rapidly:
Rapid Slump Loss: Mixes stiffen in the drum before discharge, tempting crews to add unauthorized water on site—which raises the w/cm ratio, drops 28-day strength, and causes uneven slab coloration.
Plastic Shrinkage Cracking: When surface evaporation exceeds the rate of bleed water rising to the top, hairline tears open across the slab before final finishing.
Cold Joints & Air Loss: Faster setting narrows the finishing window and makes entrained air harder to maintain.
4 Proven Controls for Summer Pours in the GTA
Schedule Early-Morning Pours: Book first-load dispatch between 6:00 AM and 8:00 AM before ambient temperatures and wind speeds peak.
Dampen Subgrade & Forms: Lightly mist granular subbases and wooden forms prior to discharge so dry stone doesn't steal mixing water from the bottom of the slab—while avoiding standing puddles.
Specify Otimo Lento & Otimo Fluxo Admixtures: Instead of adding water on site, order Otimo Lento (set-retarding admixture) to extend placement/discharge time beyond the standard 120-minute window, paired with Otimo Fluxo (high-range water reducer) for effortless pumpability at a low w/cm ratio.
Start Wet Curing Immediately: Apply fog misting, evaporation reducers during finishing, and continuous wet curing (wet burlap, sprinklers, or curing compound) immediately after bullfloating/texturing.
Planning a summer slab, bridge deck, or commercial pour? Download our CSA A23.1:24 Classes of Exposure Guide or contact ML Group dispatch at (416) 603-7878 to tailor your mix design.